About |
---|
Characteristics: High stiffness Impact strength Long term heat resistance, UL 746B Applications: Toaster Coffee Maker Steam Iron&& |
Product Description | |
---|---|
Supplier | Hyosung |
Generic | PP homopolymerization |
Material Status | Commercial: Active |
Features | High impact resistance,Good Rigidity,Heat Stabilized,Good heat aging resistance,high-rigidity |
Availabilitys | Europe,North America,Asia Pacific |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Melt Flow Rate | |||
230℃,2.16kg | 18 | g/10min | ASTM D1238 |
Density | 0.9 | g/cm³ | ASTM D792 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Flexural Modulus | 17500 | kg/cm² | ASTM D790 |
Tensile Strength | 300 | kg/cm² | ASTM D638 |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Izod Impact Strength of Cantilever Beam | |||
-10℃ | 4.0 | kgㆍcm/cm | ASTM D256 |
23℃ | 7.0 | kgㆍcm/cm | ASTM D256 |
Process Conditions | |||
---|---|---|---|
Injection molding | Nominal value | Unit | Test method |
Injection Temperature | 192-210 | ℃ | |
Injection Pressure | 600-1200 | bar |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |