About |
---|
The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM’s to get to market ahead of competition. When specified, Trilliant® compound may incorporate agency rated materials that meet USP Class IV, FDA or ISO 10993 testing requirements. This Trilliant® grade is a high density specialty compound featuring a sustainable material solution for radiation shielding and weighting & balancing applications. The composite material offers a high performance thermoplastic-based alternative to lead. This compound has densities similar to traditional metals and provides greater flexibility in design and processing.&& |
Product Description | |
---|---|
Supplier | Polyone |
Generic | PA12 |
Material Status | Commercial: Active |
Features | High density,Nontoxicity |
Availabilitys | Africa & Middle East ,North America,Latin America,Asia Pacific,Europe |
Process Methods | Injection Molding |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 11.0 | g/cm³ | ISO 1183 |
Shrinkage rate | 0.40 to 0.80 | % | ISO 294-4 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Tensile modulus | 8000 | MPa | ISO 527-1-2 |
tensile strength | |||
fracture | 45.0 | MPa | ISO 527-2/50 |
Tensile strain | |||
fracture | 0.50 to 1.0 | % | ISO 527-2/50 |
Bending modulus | 10000 | MPa | ISO 178 |
bending strength | 75.0 | MPa | ISO 178 |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Charpy Notched Impact Strength | 5.0 | kJ/m² | ISO 179 |
Charpy Unnotch Impact strength | 10 | kJ/m² | ISO 179 |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Hot deformation temperature | |||
0.45 MPa, unannealed | 160 | ℃ | ISO 75-2/B |
1.8 MPa, unannealed | 130 | ℃ | ISO 75-2/A |
Thermal conductivity coefficient | 3.0 to 3.5 | W/m/K | ASTM E1461 |
Electrical performance | Nominal value | Unit | Test method |
---|---|---|---|
Surface resistivity | < 1.0E+3 | ohms | IEC 60093 |
Process Conditions | |||
---|---|---|---|
injection | Nominal value | Unit | Test method |
Drying temperature | 80 | °C | |
Drying time | 4.0 | hr | |
Processing (melt) temperature | 230 to 280 | °C | |
Mold temperature | 65 to 100 | °C |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
2. Through Plane |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |