About |
---|
Eastman Tritan™ LX101 is an amorphous copolyester with excellent appearance and clarity. Tritan™ LX101 contains a mold release derived from vegetable based sources. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistance. Tritan™ LX101 was developed for the cosmetic, fragrance, and personal care markets. Tritan™ LX101 can easily be converted into articles for application in Consumer and Personal Care markets by injection molding, extrusion blow molding, and injection blow molding.&& |
Product Description | |
---|---|
Supplier | Eastman |
Generic | PCTG |
Material Status | Commercial: Active |
Features | Excellent Processability,Good Clarity,Good flexibility,High impact resistance,Hydrolysis stability,Quick molding cycle,Heat Resistance, Good,Solvent resistance |
Availabilitys | North America |
Process Methods | Injection Molding |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 1.18 | g/cm³ | ASTM D792 |
Shrinkage rate | |||
MD | 0.50 to 0.70 | % | ASTM D955 |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Impact strength of cantilever beam notch | ASTM D256 | ||
-40℃ | 110 | J/m | |
23℃ | 980 | J/m | |
Notched impact strength of cantilever beam | ASTM D4812 | ||
-40℃ | 无断裂 | ||
23℃ | 无断裂 | ||
Dart impact equipped with measuring instruments | ASTM D3763 | ||
-40℃ | 66.0 | J | |
23℃ | 61.0 | J |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Hot deformation temperature | ASTM D648 | ||
0.45 MPa, unannealed | 99.0 | ℃ | |
1.8 MPa, unannealed | 85.0 | ℃ |
optical performance | Nominal value | Unit | Test method |
---|---|---|---|
Transmittance | |||
total | < 90.0 | % | ASTM D1003 |
Haze | < 1.0 | % | ASTM D1003 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Rockwell hardness | |||
R-level | 112 | ASTM D785 | |
Tensile modulus | |||
23℃ | 1550 | MPa | ASTM D638 |
tensile strength | ASTM D638 | ||
Yield, 23 ℃ | 43.0 | MPa | |
Fracture, 23 ℃ | 53.0 | MPa | |
Tensile strain | ASTM D638 | ||
Yield, 23 ℃ | 6.0 | % | |
Fracture, 23 ℃ | 210 | % | |
Bending modulus | |||
23℃ | 1550 | MPa | ASTM D790 |
bending strength | |||
Yield, 23 ℃ | 62.0 | MPa | ASTM D790 |
Process Conditions | |||
---|---|---|---|
injection | Nominal value | Unit | Test method |
Drying temperature | 88.0 | °C | |
Drying time | 4.0 to 6.0 | hr | |
Processing (melt) temperature | 260 to 282 | °C | |
Mold temperature | 38.0 to 66.0 | °C |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |