ULTEM™ 1010 resin

About
ULTEM 1010 resin is an amorphous, transparent polyetherimide (PEI) plastic offering enhanced flow and a glass transition temperature (Tg) of 217°C. This inherently flame retarant resin has UL94 V0 and 5VA ratings. ULTEM 1010 resin is an unreinforced general purpose grade offering high heat resistance, high strength and modulus and broad chemical resistance up to high temperatures.&&

Product Description
SupplierSABIC
GenericPolyetherimide
Material StatusCommercial: Active
FeaturesGood Rigidity,Good liquidity,Flame Characteristics,Food contact compliance,High Heat Resistance,Solvent resistance,Amorphous,V-0,5VA
AvailabilitysNorth America,Asia Pacific,Europe
Process MethodsInjection Molding

Technical Data
PHYSICALNominal valueUnitTest method
Density1.27g/cm³ASTM D792
Melt Flow Rate
337℃,6.60kg18g/10minASTM D1238
Shrinkage rate
MD:3.2 mm0.50 to 0.70%Internal Method
Water absorption rate
Equilibrium, 23 ℃1.3%ASTM D570
24hr0.25%ASTM D570

IMPACTNominal valueUnitTest method
Impact strength of cantilever beam notch
3.2mm1200J/mASTM D256
Drop hammer impact
23℃33.9JASTM D3029

THERMALNominal valueUnitTest method
Hot deformation temperature
1.8 MPa, unannealed, 6.4 mm199ASTM D648
0.45 MPa, unannealed, 6.4 mm207ASTM D648
Vicat Softening Temp219ASTM D1525 5
Linear coefficient of thermal expansion
MD:-20~150℃5.6E-51/℃ASTM E831
Thermal conductivity coefficient0.22W/m/KASTM C177
Relative temperature index
static state170UL 746
Electrical performance170UL 746
impact strength170UL 746

Electrical performanceNominal valueUnitTest method
Volume resistivity1.0E+17ohms·cmASTM D257
Dielectric strength ASTM D149
1.6 mm in air33kV/mmASTM D149
1.6 mm in oil28kV/mmASTM D149
Dielectric constant
1 kHz3.15 ASTM D150
Dissipation factor ASTM D150
1 kHz1.3E-3 ASTM D150
2.45 GHz2.5E-3 ASTM D150
Arc resistancePLC 5 ASTM D495
Compared to the leakage tracing indexPLC 4 UL 746
High Arc Burning Index (HAI)PLC 3 UL 746
High voltage arc marking rate
HVTRPLC 2 UL 746
Hot wire ignition
HWIPLC 1 UL 746

FLAME CHARACTERISTICSNominal valueUnitTest method
Flame retardant level UL 94
0.75 mmV-0 UL 94
3.00 mm5VA UL 94
Extreme oxygen index44%ASTM D2863
Smoke density
Flame, Ds, 4 minutes2.00 ASTM E662

MECHANICALNominal valueUnitTest method
Tensile modulus3590MPaASTM D638
tensile strength
yield110MPaASTM D638
Tensile strain
fracture60%ASTM D638
yield7.0%ASTM D638
Bending modulus
100 mm span3520MPaASTM D790
bending strength
Yield, 100 mm span165MPaASTM D790
Taber abraser
1000 cycles, 1000 g, CS-17 wheels10.0mgASTM D1044
Rockwell hardness
M-level109 ASTM D785

Process Conditions
injectionNominal valueUnitTest method
Drying temperature149°C
Drying time4.0 to 6.0hr
Drying time, maximum24hr
Recommended maximum moisture content0.020%
Recommended injection volume40 to 60%
Barrel rear temperature332 to 399°C
Barrel middle temperature338 to 399°C
Barrel front temperature343 to 399°C
Nozzle temperature343 to 399°C
Processing (melt) temperature349 to 399°C
Mold temperature135 to 163°C
Back pressure0.345 to 0.689MPa
Screw speed40 to 70rpm
Vent depth0.025 to 0.076mm

Notes
1. Typical properties: these are not to be construed as specifications.
2. 0.20 in/min
3. Type I, 0.20 in/min
4. 0.10 in/min
5. Rate A (50°C/h), Loading 2 (50 N)
6. Tungsten Electrode
7. Surface
8. 4 min
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.