ULTEM™ AUT210 resin

About
ULTEM™   AUT210 resin Transparent Polyetherimide (Tg 227 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of 212 degC (SABIC IP method). Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).&&ULTEM™   AUT210 resin Transparent, Thermoplastic Polyimide (TPI). Glass transition Temperature (Tg) of 227degC. Haze onset temperature of 212degC (SABIC IP method). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Resin is a Dual-use item and is subject to export control restrictions under both U.S. 15 CFR , 774 and Annex I of Reg. (EC) 428/2009 as ECN 1C008. Diversion contrary to law is prohibited.&&

Product Description
SupplierSABIC
GenericPolyetherimide
Material StatusCommercial: Active
FeaturesLow odor
AvailabilitysNorth America,Asia Pacific,Europe
Process MethodsInjection Molding

Technical Data
PHYSICALNominal valueUnitTest method
Density1.29g/cm³ASTM D792
Density1.29g/cm³ISO 1183
Melt Flow Rate
337℃,6.60kg11g/10minASTM D1238
Melt Volume Rate
360℃,5 kg16.0cm³/10minISO 1133
Shrinkage rate
MD:3.2 mm0.50 to 0.70%Internal Method
Water absorption rate
Saturation, 23 ℃1.0%ISO 62
Equilibrium, 23 ℃, 50% RH0.20%ISO 62

MECHANICALNominal valueUnitTest method
Tensile modulus3590MPaASTM D638
Tensile modulus3320MPaISO 527-1-2
tensile strength
fracture88.0MPaASTM D638
fracture88.0MPaISO 527-2/5
yield105MPaASTM D638
yield103MPaISO 527-2/5
Tensile strain
fracture54%ISO 527-2/5
fracture75%ASTM D638
yield8.0%ASTM D638
yield7.0%ISO 527-2/5
Bending modulus3140MPaISO 178
50 mm span3330MPaASTM D790
bending strength
Yield, 50 mm span170MPaASTM D790

IMPACTNominal valueUnitTest method
Charpy Notched Impact Strength
23℃16kJ/m²ISO 179/1eA
Impact strength of cantilever beam notch ASTM D256
-30℃38J/mASTM D256
23℃37J/mASTM D256
Impact strength of cantilever beam notch ISO 180/1A
23℃2400J/mASTM D4812
-30℃4.0kJ/m²ISO 180-1A
23℃5.0kJ/m²ISO 180-1A
Notched impact strength of cantilever beam ISO 180/1U
-30℃No Break ISO 180/1U
23℃No Break ISO 180/1U
Dart impact equipped with measuring instruments
23℃,Total Energy33.0JASTM D3763

THERMALNominal valueUnitTest method
Hot deformation temperature ASTM D648
1.8 MPa, unannealed, 100 mm span196ISO 75-2/Ae
0.45 MPa, unannealed, 3.2 mm215ASTM D648
1.8 MPa, unannealed, 3.2 mm201ASTM D648
1.8 MPa, unannealed, 6.4 mm211ASTM D648
Vicat Softening Temp222ASTM D1525 9
B50221ISO 306
Linear coefficient of thermal expansion
TD:23~150℃5.0E-51/℃ISO 11359-2
TD:-40~150℃5.0E-51/℃ASTM E831
MD:23~150℃5.0E-51/℃ISO 11359-2
MD:-40~150℃5.0E-51/℃ASTM E831

Supplementary informationNominal valueUnitTest method
Metallized Haze Onset212Internal Method

Process Conditions
injectionNominal valueUnitTest method
Drying temperature149°C
Drying time4.0 to 6.0hr
Drying time, maximum24hr
Recommended maximum moisture content0.020%
Recommended injection volume40 to 60%
Barrel rear temperature360 to 382°C
Barrel middle temperature371 to 393°C
Barrel front temperature382 to 404°C
Nozzle temperature377 to 399°C
Processing (melt) temperature382 to 404°C
Mold temperature135 to 163°C
Back pressure0.345 to 0.689MPa
Screw speed40 to 70rpm
Vent depth0.025 to 0.076mm

Notes
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.