UNIGARD™ RE DFDE-1638 Natural是一种不含卤素的、阻燃性能高、热塑性、低烟、腐蚀性低和低毒性的材料。该产品是一种通用型的电缆护套材料。作为护套材料,该产品已经通过IEEE-383/UL-1581/UL-1685 [有限产烟测试] 垂直托架电缆燃烧测试。当然,电缆结构在阻燃性能方面起着重要作用。该产品可作为电缆的护套,工作温度可高达90°C。 该产品可以替代PVC、低烟PVC和含卤素橡胶作为护套材料,它具有优异的防火安全性(低烟、低腐蚀性和低毒性) 和良好的性能平衡。该产品可以满足或者超出很多业界对护套材料的规格要求,比如UL-1277 托架电缆的规格要求。 作为一种不含卤素的阻燃护套材料,UNIGARD™ RE DFDE-1638 Natural也可用于替代普通的非卤素护套产品。与现有的非卤素护套产品相比,这种产品的挤出温度最高到180°C,而且可以使用常用的单螺线计量PE螺杆进行挤出加工。 主要特性: 阻燃级别高 环保 (无铅、不含卤素、无硫/无锑) 低烟、腐蚀性低以及低毒性 挤出容易,无需特殊螺杆 在韧性和柔软性之间具有良好的平衡性&&

Product Description
SupplierDOW
Generic热塑性聚酯
Material StatusCommercial: Active
AvailabilitysAfrica & Middle East ,North America,Latin America,Asia Pacific,Europe

Technical Data
PHYSICALNominal valueUnitTest method
Density1.48g/cm³ASTM D1505
ESCR(Environmental Stress Cracking Resistance)
10% non-ionic detergent, F0720hrASTM D1693

elastic bodyNominal valueUnitTest method
tear strength6.13kN/mASTM D470

Aging performanceNominal valueUnitTest method
Tensile strength retention rateASTM D638
10 days:110℃110%
7 days:121℃110%
Elongation retention rateASTM D638
10 days:110℃78%
7 days:121℃80%

THERMALNominal valueUnitTest method
Embrittlement temperature-24.0ASTM D746
thermal deformationUL 1581
90℃4.0%
100℃4.0%
121℃20%

Electrical performanceNominal valueUnitTest method
Volume resistivity
23℃1.9E+15ohms·cmASTM D257
Dielectric constant
60 Hz3.90ASTM D1531
Dissipation factor
60 Hz0.013ASTM D1531

FLAME CHARACTERISTICSNominal valueUnitTest method
Extreme oxygen index35%ASTM D2863
Acid gas test
Acid by Weight%MIL C-24643
toxicity0.900NES 713
Acid gas emission pH4.40IEC 60754-2
Conductivity of acidic gas emissions29.0µS/cmIEC 60754-2
Temperature index (combustion) – Critical> 300NES 715
smoke13.7NES 711
Smoke densityASTM E662
Flaming Mode – D1.5:2.54 mm0.40
Flaming Mode – D4.0:2.54 mm51
Flaming Mode – Dm,corr.:2.54 mm320
Non combustion mode – D1.5:2.54 mm0.10
Non combustion mode – D4.0: 2.54 mm12
Non-flaming Mode – Dm, corr.:2.54 mm 9190

Supplementary informationNominal valueUnitTest method
Sunshine resistant
720 hours通过UL 1581
memo_intro

MECHANICALNominal valueUnitTest method
Shore hardness
Shaw’s A96ASTM D2240
tensile strength14.7MPaASTM D638
Tensile strain
fracture150%ASTM D638
Bending modulus
1% secant138MPaASTM D790

Notes
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.