VESTAMID® HTplus M1000

About
Unmodified polyphthalamide for creating compounds for injection molding VESTAMID HTplus M1000 is a neat resin for polyphthalamide (PPA) based compounds for injection molding. This base resin is especially suitable for manufacturing parts subjected to high temperature.&&

Product Description
SupplierEvonik
GenericPPA
Material StatusCommercial: Active
FeaturesHigh Heat Resistance
AvailabilitysNorth America,Europe
Process MethodsInjection Molding

Technical Data
PHYSICALNominal valueUnitTest method
Density1.20g/cm³ISO 1183

MECHANICALNominal valueUnitTest method
Tensile modulus3500MPaISO 527-2
tensile strength
fracture90.0MPaISO 527-2
Tensile strain
fracture3.0%ISO 527-2

IMPACTNominal valueUnitTest method
Charpy Notched Impact Strength ISO 179/1eA
-40 ℃, completely fractured4.0kJ/m²ISO 179/1eA
23 ℃, completely fractured7.0kJ/m²ISO 179/1eA
Charpy Unnotch Impact strength ISO 179/1eU
-40 ℃, completely fractured40kJ/m²ISO 179/1eU
23 ℃, completely fractured50kJ/m²ISO 179/1eU

THERMALNominal valueUnitTest method
Hot deformation temperature
1.8 MPa, unannealed126ISO 75-2/A
0.45 MPa, unannealed223ISO 75-2/B
Vicat Softening Temp 
302ISO 306/A
223ISO 306/B
Melting temperature300 to 315ISO 11357-3

Process Conditions
injectionNominal valueUnitTest method
Drying temperature120°C
Drying time4.0hr

Notes
1. Typical properties: these are not to be construed as specifications.
2. 2nd heating
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.