Visico™ FR4450/LE4439

About
Visico FR4450/LE4439 is a scorch retardant, moisture-crosslinking polyethylene compound for low voltage insulation. FR4450/LE4439 is a natural, zero halogen, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The combination of a VISICO FR4450 base resin, and the LE4439 catalyst, provides a highly scorch retardant compound with excellent thermal stability and good retardant flame properties. FR4450/LE4439 contains a patented scorch retardant additive (SRA) that increases the processing window for a moisture crosslinking compound and minimizes the tendency for premature crosslinking in the extruder, head or die. A finished compound that is composed of 95 parts of FR4450 mixed with 5 parts of LE4439 is recognized by Underwriters Laboratories as VISICO FR4450/LE4439 95/5. FR4450/LE4439 is designed to reduce normal PE flame spread characteristics and achieve an HB-1 flame rating on 14 AWG wires and larger. LE4439 also provides, in addition to catalyst, a stabilization package containing suitable antioxidants, a metal passivator and a metal deactivator. Properly mixed, during the extrusion process, FR4450/LE4439 exhibits excellent thermal stability to oxidation. FR4450/LE4439 is readily pigmented to a variety of colors using standard wire & cable color concentrates designed for thermoplastic or crosslinked polyethylene. Application FR4450/LE4439 is recommended for use as insulation and sheath for low voltage control cables and power cables up to 6kv in rating. Specifications UL 44&&

Product Description
SupplierBorealis AG
GenericPE
Material StatusCommercial: Active
FeaturesCrosslinked,Halogen free,Flame Characteristics,Inoxidizability,Heat Stabilized,Good coloring
AvailabilitysAfrica & Middle East ,North America,Latin America,Asia Pacific,Europe

Technical Data
PHYSICALNominal valueUnitTest method
Density
0.940g/cm³
1.10g/cm³
Melt Flow Rate
190℃,2.16kg0.70g/10minASTM D1238

elastic bodyNominal valueUnitTest method
tensile strengthMPaASTM D412
Tensile strain
fracture> 300%ASTM D412

THERMALNominal valueUnitTest method
High temperature creep
Elongation under load: 150 ℃< 50%
Permanent deformation: 150 ℃< 5.0%

Electrical performanceNominal valueUnitTest method
Volume resistivity> 1.0E+16ohms·cmASTM D257
Dielectric strength> 22kV/mmASTM D149
Dielectric constant
50 Hz< 3.00 ASTM D150
Dissipation factor< 2.0E-3 ASTM D150

FLAME CHARACTERISTICSNominal valueUnitTest method
Extreme oxygen index32%ASTM D2863
Corrosive gases in flue gas15.0µS/cmIEC 60754-2

Supplementary informationNominal valueUnitTest method
Horizontal Flame Test(14 AWG,762.0 µm)Pass UL 44

Process Conditions
ExtrusionNominal valueUnitTest method
Barrel 1 zone temperature140°C
Barrel 2 zone temperature140°C
Barrel 3 zone temperature150°C
Barrel 4 zone temperature160°C
Barrel 5 zone temperature170°C

Notes
1. Typical properties: these are not to be construed as specifications.
2. LE4439
3. Visico FR4450
4. 0.20 MPa
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.