Vydyne® 75HF

About
Vydyne 75HF is a medium-high-viscosity, heat-stabilized PA66/6 copolymer resin designed for extrusion applications. This product is available in natural only. It offers a well-balanced combination of engineering properties characterized by high melt point; high strength and rigidity; good toughness; soft hand and good chemical resistance.&&

Product Description
SupplierAscend
GenericPA66/6
Material StatusCommercial: Active
FeaturesGood Rigidity,Good flexibility,High molecular weight,Grease resistance,Solvent resistance,Gasoline resistance,Heat Stabilized,Higher melt stability
AvailabilitysNorth America,Asia Pacific,Europe
Process MethodsExtrusion

Technical Data
PHYSICALNominal valueUnitTest method
Density1.14g/cm³ISO 1183
Water absorption rate
Saturation, 23 ℃8.5%ISO 62
Equilibrium, 23 ℃, 50% RH2.5%ISO 62

MECHANICALNominal valueUnitTest method
Tensile modulus
23℃2700MPaISO 527-2
tensile strength ASTM D882
Fracture, 23 ℃50.0MPaISO 527-2
Yield, 23 ℃80.0MPaISO 527-2
TD, fracture, blow molded film105MPaASTM D882
MD, fracture, blow molded film121MPaASTM D882
Ultimate105MPaASTM D882
Ultimate123MPaASTM D882
Nominal tensile fracture strain
23℃> 200%ISO 527-2
Bending modulus
23℃2200MPaISO 178
bending strength
23℃70.0MPaISO 178
Poisson’s ratio0.40 ISO 527-2

filmNominal valueUnitTest method
Secant modulus
1% secant, TD, cast thin film444MPaASTM D882
1% secant, MD, cast thin film392MPaASTM D882
Tensile strain
Yield, 23 ℃5.0%ISO 527-2
TD, fracture, cast thin film500%ASTM D882
TD, yield, cast thin film6.7%ASTM D882
MD, fracture, extruded film450%ASTM D882
MD, yield, cast thin film7.0%ASTM D882
Drop hammer impact
42 µ m, cast thin film> 2100gASTM D1709
tear strength
TD, 42 µ m, cast thin film110gASTM D1922
MD, 42 µ m, cast thin film100gASTM D1922

IMPACTNominal valueUnitTest method
Charpy Notched Impact Strength ISO 179/1eA
-30℃8.0kJ/m²ISO 179/1eA
23℃4.0kJ/m²ISO 179/1eA
Charpy Unnotch Impact strength ISO 179/1eU
-30℃No Break ISO 179/1eU
23℃No Break ISO 179/1eU
Impact strength of cantilever beam notch ISO 180
-30℃8.0kJ/m²ISO 180
23℃4.0kJ/m²ISO 180

THERMALNominal valueUnitTest method
Hot deformation temperature
1.8 MPa, unannealed45.0ISO 75-2/A
0.45 MPa, unannealed125ISO 75-2/B
Melting temperature220ISO 11357-3
Linear coefficient of thermal expansion
TD:23~55℃,2 mm1.0E-41/℃ISO 11359-2
MD:23~55℃,2 mm1.0E-41/℃ISO 11359-2

Process Conditions
ExtrusionNominal valueUnitTest method
Barrel 1 zone temperature230 to 275°C
Barrel 2 zone temperature230 to 275°C
Barrel 3 zone temperature230 to 275°C
Barrel 4 zone temperature230 to 275°C
Barrel 5 zone temperature230 to 275°C
Melt temperature235 to 275°C
Nozzle temperature240°C

Notes
1. Typical properties: these are not to be construed as specifications.
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.