XENOY™ 5720U resin

About
Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY&&

Product Description
SupplierSABIC
GenericPC+PBT
Material StatusCommercial: Active
FeaturesWeather resistance is good,Solvent resistance,low-temperature impact resistance
AvailabilitysNorth America,Asia Pacific,Europe
Process MethodsInjection Molding

Technical Data
PHYSICALNominal valueUnitTest method
Density1.17g/cm³ASTM D792
Specific volume0.850cm³/gASTM D792
Density1.17g/cm³ISO 1183
Melt Flow Rate ASTM D1238
250℃,2.16kg3.8g/10minASTM D1238
250℃,5.0kg11g/10minASTM D1238
265℃,2.16kg6.8g/10minASTM D1238
266℃,5.0kg20g/10minASTM D1238
Melt Flow Rate ISO 1133
250℃,2.16kg3.8g/10minISO 1133
250℃,5.0kg11g/10minISO 1133
Melt Volume Rate ISO 1133
250℃,2.16 kg3.60cm³/10minISO 1133
250℃,5 kg10.9cm³/10minISO 1133
265℃,2.16 kg6.50cm³/10minISO 1133
265℃,5 kg18.9cm³/10minISO 1133
Shrinkage rate
MD:3.2 mm1.0 to 1.2%Internal Method
Water absorption rate
Saturation, 23 ℃0.28%ISO 62
Equilibrium, 23 ℃, 50% RH0.080%ISO 62

MECHANICALNominal valueUnitTest method
Tensile modulus 
1830MPaASTM D638
1830MPaInternal Method
1820MPaASTM D638
Tensile modulus1800MPaISO 527-1-2
tensile strength 
yield44.0MPaASTM D638
yield45.0MPaInternal Method
yield47.0MPaASTM D638
tensile strength 
yield44.0MPaISO 527-2/5
yield47.0MPaISO 527-2/50
tensile strength 
fracture50.0MPaASTM D638
fracture47.0MPaInternal Method
fracture48.0MPaASTM D638
tensile strength 
fracture43.0MPaISO 527-2/5
fracture43.0MPaISO 527-2/50
Tensile strain 
yield4.6%ASTM D638
yield4.6%Internal Method
yield4.0%ASTM D638
Tensile strain 
yield4.1%ISO 527-2/5
yield4.6%ISO 527-2/50
Tensile strain 
fracture120%ASTM D638
fracture110%Internal Method
fracture120%ASTM D638
Tensile strain 
fracture110%ISO 527-2/5
fracture120%ISO 527-2/50
Bending modulus1870MPaISO 178
50 mm span1660MPaASTM D790
bending strength71.0MPaISO 178
bending strength
Fracture, 50 mm span69.0MPaASTM D790
Yield, 50 mm span70.0MPaASTM D790

IMPACTNominal valueUnitTest method
Charpy Notched Impact Strength ISO 179/1eA
-30℃48kJ/m²ISO 179/1eA
23℃56kJ/m²ISO 179/1eA
Impact strength of cantilever beam notch ASTM D256
-40℃600J/mASTM D256
-30℃650J/mASTM D256
-20℃700J/mASTM D256
-10℃660J/mASTM D256
0℃690J/mASTM D256
23℃720J/mASTM D256
Impact strength of cantilever beam notch ISO 180/1A
-40℃46kJ/m²ISO 180-1A
-30℃48kJ/m²ISO 180-1A
-20℃50kJ/m²ISO 180-1A
-10℃52kJ/m²ISO 180-1A
0℃55kJ/m²ISO 180-1A
23℃56kJ/m²ISO 180-1A
Dart impact equipped with measuring instruments ASTM D3763
-40℃,Energy at Peak Load49.5JASTM D3763
-40℃,Total Energy59.2JASTM D3763
-30℃,Energy at Peak Load49.5JASTM D3763
-30℃,Total Energy61.9JASTM D3763
-20℃,Energy at Peak Load41.9JASTM D3763
-20℃,Total Energy53.2JASTM D3763
23℃,Energy at Peak Load44.8JASTM D3763
23℃,Total Energy54.0JASTM D3763

THERMALNominal valueUnitTest method
Hot deformation temperature ASTM D648
0.45 MPa, unannealed, 3.2 mm108ASTM D648
0.45 MPa, unannealed, 6.4 mm117ASTM D648
Hot deformation temperature ASTM D648
1.8 MPa, unannealed, 64 mm span87.0ISO 75-2/Af
0.45 MPa, unannealed, 64 mm span110ISO 75-2/Bf
1.8 MPa, unannealed, 3.2 mm83.5ASTM D648
1.8 MPa, unannealed, 6.4 mm95.9ASTM D648
Vicat Softening Temp120ASTM D1525 14
Vicat Softening Temp 
B50120ISO 306
B120122ISO 306/B120
Linear coefficient of thermal expansion
TD:-40~95℃1.0E-41/℃ASTM E831
TD:-30~80℃1.0E-41/℃ISO 11359-2
MD:-40~95℃9.8E-51/℃ASTM E831
MD:-30~80℃9.8E-51/℃ISO 11359-2

Process Conditions
injectionNominal valueUnitTest method
Drying temperature110°C
Drying time4.0 to 6.0hr
Drying time, maximum8.0hr
Recommended maximum moisture content0.020%
Recommended injection volume50 to 80%
Barrel rear temperature243 to 266°C
Barrel middle temperature249 to 271°C
Barrel front temperature254 to 277°C
Nozzle temperature254 to 271°C
Processing (melt) temperature260 to 277°C
Mold temperature66 to 88°C
Back pressure0.345 to 0.689MPa
Screw speed50 to 80rpm
Vent depth0.013 to 0.020mm

Notes
1. Typical properties: these are not to be construed as specifications.
2. 0.20 in/min
3. 0.39 in/min
4. 2.0 in/min
5. Type I, 2.0 in/min
6. Type I, 0.39 in/min
7. Type I, 0.20 in/min
8. 0.051 in/min
9. 0.079 in/min
10. Yield
11. 80*10*4 sp=62mm
12. 80*10*4
13. 80*10*4 mm
14. Rate B (120°C/h), Loading 2 (50 N)
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.