XYLEX™ X8210 resin

About
PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility&&

Product Description
SupplierSABIC
GenericPC + Polyester
Material StatusCommercial: Active
FeaturesGood Clarity,High impact resistance,Ductility
AvailabilitysNorth America,Europe
Process MethodsInjection Molding

Technical Data
PHYSICALNominal valueUnitTest method
Density1.20g/cm³ASTM D792
Density1.16g/cm³ISO 1183
Melt Flow Rate ASTM D1238
265℃,2.16kg10g/10minASTM D1238
300℃,1.20kg14g/10minASTM D1238
Melt Volume Rate ISO 1133
265℃,2.16 kg10.0cm³/10minISO 1133
300℃,1.2 kg13.0cm³/10minISO 1133
Shrinkage rate
TD:3.2 mm0.40 to 0.60%Internal Method
MD:3.2 mm0.50 to 0.80%Internal Method
Water absorption rate
Saturation, 23 ℃0.37%ISO 62
Equilibrium, 23 ℃, 50% RH0.15%ISO 62

MECHANICALNominal valueUnitTest method
Tensile modulus1480MPaASTM D638
Tensile modulus1500MPaISO 527-1-2
tensile strength
fracture45.0MPaISO 527-2/50
fracture46.0MPaASTM D638
yield45.0MPaISO 527-2/50
yield43.0MPaASTM D638
Tensile strain
fracture> 150%ISO 527-2/50
fracture150%ASTM D638
yield5.0%ASTM D638
yield4.6%ISO 527-2/50
Bending modulus1600MPaISO 178
50 mm span1600MPaASTM D790
bending strength58.0MPaISO 178
bending strength
Yield, 50 mm span65.0MPaASTM D790

IMPACTNominal valueUnitTest method
Charpy Notched Impact Strength
23℃71kJ/m²ISO 179/1eA
Impact strength of cantilever beam notch ASTM D256
-30℃200J/mASTM D256
-20℃640J/mASTM D256
23℃800J/mASTM D256
Impact strength of cantilever beam notch ISO 180/1A
-30℃11kJ/m²ISO 180-1A
-10℃30kJ/m²ISO 180-1A
23℃45kJ/m²ISO 180-1A
Dart impact equipped with measuring instruments
23℃,Total Energy81.0JASTM D3763

THERMALNominal valueUnitTest method
Hot deformation temperature 
1.8 MPa, unannealed, 3.2 mm75.0ASTM D648
0.45 MPa, unannealed, 3.2 mm79.0ASTM D648
1.8 MPa, unannealed, 100 mm span82.0ISO 75-2/Ae
1.8 MPa, unannealed, 64 mm span81.0ISO 75-2/Af
Vicat Softening Temp97.0ASTM D1525 11
Vicat Softening Temp 
B5092.0ISO 306
B12097.0ISO 306/B120
Linear coefficient of thermal expansion
TD:-40~40℃8.9E-51/℃ISO 11359-2
TD:-40~40℃1.1E-41/℃ASTM E831
MD:-40~40℃1.1E-41/℃ASTM E831
MD:-40~40℃8.3E-51/℃ISO 11359-2

optical performanceNominal valueUnitTest method
Transmittance
2540 µm85.0%ASTM D1003
Haze
2540 µm4.0%ASTM D1003

Process Conditions
injectionNominal valueUnitTest method
Drying temperature66 to 77°C
Drying time3.0 to 5.0hr
Drying time, maximum8.0hr
Recommended maximum moisture content0.020%
Recommended injection volume40 to 80%
Barrel rear temperature238 to 249°C
Barrel middle temperature238 to 260°C
Barrel front temperature243 to 266°C
Nozzle temperature243 to 266°C
Processing (melt) temperature243 to 266°C
Mold temperature43 to 60°C
Back pressure0.172 to 0.517MPa
Screw speed20 to 100rpm
Vent depth0.013 to 0.020mm

Notes
1. Typical properties: these are not to be construed as specifications.
2. 2.0 in/min
3. Type I, 2.0 in/min
4. 0.051 in/min
5. 0.079 in/min
6. at Break
7. 80*10*4 sp=62mm
8. 80*10*4 mm
9. 120*10*4 mm
10. Rate A (50°C/h), Loading 2 (50 N)
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.