Product Description | |
---|---|
Supplier | DuPont |
Generic | PA66/6 |
Material Status | Commercial: Active |
Process Methods | Injection Molding |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 1.39 | g/cm³ | ISO 1183 |
Shrinkage rate | |||
TD | 0.8 | % | ISO 294-4 |
MD | 0.2 | % | ISO 294-4 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
tensile strength | |||
fracture | 184 | MPa | ISO 527-1/-2 |
Tensile modulus | 9300 | MPa | ISO 527-1/-2 |
Tensile strain | |||
fracture | 3.3 | % | ISO 527-1/-2 |
bending strength | 288 | MPa | ISO 178 |
Bending modulus | 9070 | MPa | ISO 178 |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Charpy Unnotch Impact strength | |||
23℃ | 95 | kJ/m² | ISO 179/1eU |
Charpy Notched Impact Strength | |||
23℃ | 25 | kJ/m² | ISO 179/1eA |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Hot deformation temperature | |||
1.80 MPa | 225 | ℃ | ISO 75-1/-2 |
FLAME CHARACTERISTICS | Nominal value | Unit | Test method |
---|---|---|---|
Flame retardant level | |||
1.5 mm | HB | IEC 60695-11-10 | |
0.8 mm | HB | IEC 60695-11-10 | |
FMVSS | B | ISO 3795 |
Process Conditions | |||
---|---|---|---|
injection molding | Nominal value | Unit | Test method |
drying temperature | 85 | ℃ | |
Drying time | 3-4 | hrs | |
Melt processing temperature | 290-310 | ℃ | |
Mold temperature | 65-120 | ℃ |
Notes |
---|
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |